Choosing the wrong class is the most expensive mistake: the tile comes loose a few months later and the whole covering has to come off. The selector below shows the required class and the matching ZNR products in three questions.
The most expensive mistake in choosing an adhesive is the wrong class: the tile comes loose a few months later.
| Code | What | Explanation |
|---|---|---|
| C2 | Yapışma sınıfı | C1 normal, C2 geliştirilmiş yapışma. Emici olmayan karoda ve dış mekanda C2 istenir. |
| T | Kayma direnci | Düşey yüzeyde karonun aşağı kaymaması. Duvar uygulamasında aranır. |
| E | Uzatılmış açık zaman | Harç sürüldükten sonra karonun yapıştırılabileceği sürenin uzun olması. Sıcakta ve büyük alanda kritik. |
| S1 | Deformasyon sınıfı | S1 esnek, S2 yüksek esnek. Yerden ısıtma, dış mekan ve büyük ebat karoda gerekir. |
This page is not a layer build-up but a selection guide; which product to choose is determined by the class above. The whole TILE, CERAMIC, MARBLE, GRANITE, NATURAL STONE ADHESIVES AND GROUTS group is listed in the catalogue.
TILE, CERAMIC, MARBLE, GRANITE, NATURAL STONE ADHESIVES AND GROUTS ürünleriYes. 6 mm for small tiles, 8-10 mm for medium sizes, 12 mm and above for large formats. As the notch grows, consumption increases almost linearly; between 6 mm and 12 mm the difference is more than double.
It is not. For tiles over 60 cm the adhesive is applied both to the substrate and to the back of the tile. The aim is contact without voids; a void underneath leads both to breakage and to water collecting in wet areas.
It can, but class C2 is essential. Since the old surface is not absorbent there is no mechanical keying; adhesion is entirely chemical. The surface must also be cleared of grease and polishes.
The joint is the only place that absorbs the thermal and moisture-driven movement of the tiles. With zero joints the movement is taken by the tile itself and lifting starts at the edges. Joint width is set according to tile size.
Details such as the parapet return, the drain mouth and the expansion joint decide the fate of the system. Our technical team looks at it in place.