What finishes a car park floor is not the load but the kind of load. Tyre marks, the lateral force of braking and turning, drops of fuel and antifreeze, salt water carried in during winter — concrete on its own stands up to none of these. The surface dusts, the coating lifts, water reaches the reinforcement.
4 layers, in application order.
| Layer | Product | Role | Consumption and packaging | |
|---|---|---|---|---|
| 01 | Surface preparation and repair |
ZNR REPAIR C5
303
|
Blowholes, cracks and level differences after shot blasting. When required. |
2.00 kg/m² for 1 mm thickness
25 kg kraft bag
|
| 02 | Primer |
ZNR PRIMER EP
407
|
Fills the pores and establishes the adhesion of the body coat. Mandatory. If surface moisture is above 4%, use 405 ZNR 501 C. |
150–300 g/m² (Varies depending on surface conditions)
20 kg Set (A: 14 kg + B: 6 kg)
|
| 03 | Body coat |
ZNR SELF LEVELING FLORING EP-2K
410
|
Self-leveling epoxy, 2 mm. The layer that carries the load and provides the seal. Mandatory.
⚠ a site–TDS difference for consumption is awaiting a decision |
1.20–1.40 kg/m² for 1 mm thickness
(Varies depending on surface conditions)
20 kg Set (A: 16 kg + B: 4 kg)
|
| 04 | UV-resistant topcoat |
ZNR PUSO 650 XH
417
|
Aliphatic polyurethane, 2 coats. Prevents UV yellowing and cracking from thermal movement. Mandatory on open decks. |
0.150–0.250 kg/m² in a single coat
(Varies depending on surface conditions)
20 kg Set
(A: 18.2 kg + B: 1.8 kg)
|
Consumption and packaging are read from the product record and are not written separately on this page — when the product is updated, this is updated too.
4 products. The other items in the system (insulation board, dowel, drainage board, mechanical work) are not ZNR products and are not in the catalogue.

Shrinkage-Free Cement-Based Structural Fine Repair Mortar

Solvent-Free Impregnation Epoxy Primer

Self-Leveling Solvent-Free Epoxy Coating

Aliphatic Polyurethane Topcoat Paint
It should not be. If the moisture content of the concrete is above 4% by weight, a standard epoxy primer will not hold and the coating blisters within a few months. In that case the moisture-tolerant 405 ZNR 501 C is used.
It is not. Acid does not remove the laitance completely and leaves salts on the surface. An open-pored surface must be obtained by shot blasting or grinding; adhesion depends on it.
No. On ramps and turning areas braking and lateral forces are high; a broadcast anti-slip quartz is mandatory and consumption comes out close to the upper limit.
It is not. On a surface that never sees the sun an aliphatic topcoat is an added cost. However, where the entrance ramp and the open edges receive daylight, it is applied to those areas.
Details such as the parapet return, the drain mouth and the expansion joint decide the fate of the system. Our technical team looks at it in place.